Fabric Sourcing for Garment Buyers: Guides and Specifications

Fabric is where most garment programmes quietly fail. The sample is approved on a swatch, the bulk arrives on a different lot, and the shade, hand-feel or shrinkage no longer matches the spec. Everything else in this hub follows from that risk.

What to lock before you place an order

  • Composition and yarn count — written as percentages with a tolerance, not as a trade name.
  • Weight (GSM) and width — with the measurement method stated, because GSM measured on greige and on finished fabric differ.
  • Shrinkage after wash — the single most common cause of a failed bulk delivery.
  • Colour fastness — to washing, rubbing and light, with the standard named (ISO or AATCC).
  • Hand-feel reference — a physical retained swatch, signed by both sides, beats any adjective.

The guides

Why fabric sets the MOQ

A factory can cut 50 pieces of a garment. A mill will not weave or knit 50 metres of a custom fabric. That is why the minimum order conversation usually starts with the fabric specification, not with the garment: the moment you choose a custom dye lot, the mill minimum becomes your floor.

If you want a low minimum, the practical route is a stock fabric in a standard colourway, with your differentiation coming from the pattern, trims and finishing. If the fabric is the product, plan the programme around the mill minimum instead.

The specification sheet: fields that decide acceptance

FieldWhy it decides the outcomeHow to write it
Fibre compositionDrives price, hand-feel and care labellingPercentages with a tolerance, e.g. 95% cotton / 5% elastane ±2%
ConstructionSingle jersey, rib, interlock, twill, dobby — not interchangeableName the construction plus yarn count
WeightDetermines drape and whether the garment holds shapeGSM with the state measured: greige, finished or washed
WidthSets marker efficiency and therefore fabric consumptionUsable width in cm, tube or open width
ShrinkageThe most common reason a bulk delivery is rejected% length and width after a named wash cycle
Colour fastnessDecides whether the garment survives its first customer washGrade against ISO 105 or AATCC, per condition
Hand-feel referenceAdjectives do not travel; swatches doA retained, signed swatch held by both sides

Testing to request before bulk

  • Shrinkage after three washes — not one. Most relaxation happens in the first two cycles.
  • Colour fastness to washing, rubbing and light — the three that generate returns.
  • Pilling — especially on wool blends and low-twist yarns; grade it rather than describing it.
  • Dimensional stability of the seam — a fabric that passes flat can still pucker at the seam after wash.
  • Substance check against the approved lot — weight drift between lots is common and rarely volunteered.

Where fabric sourcing goes wrong

The typical failure is not a bad mill. It is an approved swatch that never became a written specification, followed by a bulk lot that meets the mill’s own standard rather than the buyer’s. The second most common failure is a last-minute colour change that moves the order to a different dye lot, and with it the hand-feel the sample was approved on. Both are prevented by the same discipline: every attribute that matters is written down, measured the same way on both sides, and tied to a retained physical reference.

Cogarm has manufactured custom knitwear and woven garments in Dongguan, Guangdong, China since 2006. Minimum order is 100 units per style and colourway.

Leave a Reply